Unlike an oscillating-disc rheometer (ODR), the MDR uses a sealed, rotorless die cavity. With no embedded rotor to heat, the specimen reaches test temperature faster and more uniformly, temperature recovery after loading is short, and cured samples are easier to remove. The result is excellent repeatability and reproducible cure data from batch to batch and from lab to lab.
ASTM D5289 - Standard Test Method for Rubber Property-Vulcanization Using Rotorless Cure Meters (current edition)
ISO 6502-3:2023 - Rubber - Measurement of vulcanization characteristics using curemeters - Part 3: Rotorless curemeter (general guidance: ISO 6502-1)
An uncured rubber specimen (typically 4-5 cm³, cut with a volumetric sample cutter) is placed between two heated dies forming a sealed, nearly closed cavity, and held at the set test temperature. The lower die oscillates through a small sinusoidal angular arc (standard ±0.5°, optional ±1° or ±3°) at 1.67 Hz (100 cpm), applying a defined oscillatory shear strain to the compound.
The torque transmitted to the stationary die is measured by a high-resolution load cell and recorded as a function of time. As the compound warms and softens, torque falls to its minimum ML (compound viscosity). Once crosslinking starts, torque rises through the scorch point to a plateau or maximum MH (crosslink density / cured stiffness). Compounds prone to reversion show a torque drop after the peak. The resulting torque-time curve (cure curve), together with the temperature curve, is displayed live and stored automatically; its shape depends on the test temperature and on the compound's formulation.
| Item | Specification |
| Temperature range | Ambient to 200 °C |
| Temperature fluctuation | ±0.15 °C |
| Temperature display resolution | 0.01 °C |
| Heating rate | Approx. 15 °C/min |
| Temperature recovery time | < 1.5 min |
| Temperature units | °C, °F, K |
| Torque range | 0-20 N·m (0-200 dN·m) |
| Torque minimum reading / resolution | 0.001 N·m |
| Torque accuracy | ±0.3 % FS |
| Oscillation amplitude | ±0.5° standard; ±1°, ±3° optional |
| Oscillation frequency / speed | 1.67 Hz (100 cpm / 100 r/min) |
| Data acquisition rate | 200 samples/s (200 Hz) |
| Calculated parameters | ts1, ts2, t10, t30, t50, t70, t90, Vc1, Vc2 |
| Report / print contents | Date, time, temperature, cure curve, temperature curve, ML, MH, ts1, ts2, t10, t30, t50, t70, t90, Vc1, Vc2 |
| Torque units | N·m, dN·m, N·cm, N·in, kN·m, kN·cm, kN·in, kgf·m, kgf·cm, kgf·in, lbf·m, lbf·cm, lbf·in, gf·m, gf·cm, gf·in |
Compound development: evaluating cure packages, accelerators, fillers and anti-scorch agents
Batch-to-batch QC and release testing of mixed rubber compounds
Setting press cure times for compression, transfer and injection molding; avoiding under-cure and over-cure
Tyres, seals & gaskets, hoses & belts, vibration mounts, footwear, wire & cable compounds
Incoming material inspection, supplier qualification and third-party test laboratories
A stable single-phase 220 V / 50 Hz supply and clean compressed air at 0.5-0.65 MPa are required; the user supplies an 8 mm OD air tube. Use protective polyester/nylon film and a constant-volume specimen cutter for repeatable results. Allow the dies to stabilise at the set temperature before starting a test.
Q: What is the difference between an MDR and an ODR?
A: An MDR has no rotor embedded in the specimen. Heating is faster and more uniform, temperature recovery is shorter, and samples are easier to remove. Results from the two instrument types are not directly interchangeable - establish a correlation before transferring QC limits.
Q: Which standard should I follow
A: ASTM D5289 and ISO 6502-3:2023 are the common methods for rotorless curemeters; DIN 53529 and GB/T 9869.3-2025 may be required by regional customers. Agree the standard, test temperature, oscillation arc and frequency with your customer before testing.
Q: What affects repeatability most?
A: Sample volume and conditioning, die cleanliness/seal condition, and temperature recovery after loading. Use a volumetric cutter and keep the same rest time between mixing and testing.